I also came across the zinc interleaves but not too keen on those either !
However I did find out that modern restorers of (I think) MGs use a circa 1mm hard plastic sheet instead of the zinc interleaves and this works just as well. It might be worth researching this possibility if you are interested.
Zinc interleaves can tend to corrode when water gets in which is the reason I did not use them.